I am trying to colour-match the gel coat on my 1992 OUTRAGE 17, but in the United Kingdom everything is difficult to get, and I cannot get international postage for the Spectrum patch kit.

Q1: how can I get color-match gel coat repair paste in the United Kingdom?

jimh
Posts: 13285
Joined: Fri Oct 09, 2015 12:25 pm
Location: Michigan, Lower Peninsula
Contact:

Re: Source for Color-Matched Gel Coat Resin in the United Kingdom

Postby jimh » Tue Feb 17, 2026 10:09 am

Perhaps if you contact a Boston Whaler dealer in the USA that has a great parts department, you could arrange for them to send you some color-match gel coat repair paste.

For starters, you might try contacting Sue Lodel via email. For her contact information see

Latest Sue Lodel Contact Information
https://continuouswave.com/forum/viewto ... 06l#p46706

Another alternative: contact a Boston Whaler dealer in the United Kingdom.

Also possible: make your own polyester resin gel coat by tinting white resin with very small amounts of acrylic paint pigments. To help the resin cure use a top coat of poly-vinyl alcohol. I give a detailed first hand account of how to do this in an article I wrote many years ago. See

Minor Repairs with Epoxy
https://continuouswave.com/maintenance-logs/epoxy/

AlastairOR17
Posts: 2
Joined: Mon Feb 16, 2026 11:12 am

Re: Source for Color-Matched Gel Coat Resin in the United Kingdom

Postby AlastairOR17 » Thu Jun 18, 2026 6:11 pm

Thanks for the reply, much appreciated. I tried the [the suggestions to buy the resin in the USA] and no one would ship internationally. I ended up paying a local guy to colour match a couple of litres by eye, and he’s done an amazing job. The restoration is coming along really well now and I have some spare resin.